AimsBefore you startIntroductionBasic principlesThermodynamics and kineticsPrimary batteriesZinc/carbon batteriesAlkaline/manganese oxide batteriesZinc/silver oxide batteriesSecondary batteriesLead/acid batteriesLithium batteriesBattery characteristicsThe futureQuestionsGoing furtherTLP creditsTLP contentsShow all contentViewing and downloading resourcesAbout the TLPsTerms of useFeedbackCredits Print this page
PreviousNext
Introduction
Electrical energy/power storage has widespread applications as can be seen in the sheer range and diversity of batteries used as a source of electrical power. Batteries range from tiny button cells storing miliwatthours of energy and delivering microwatt power, to gigantic load levelling batteries situated within a factory size building, storing megawatthours of energy and delivering megawatts of power.