2 videos for category Microstructural animations:
Image
![]() |
video 143 : Changes in microstructure of a shape memory alloy being heat treated and also mechanically deformed. From TLP: Superelasticity and Shape Memory Alloys Videos kindly donated by Vaclav Novak and Per Sittner Department of Functional Materials Institute of Physics of the ASCR, Prague Czech Republic |
Image
![]() |
video 144 : Changes in microstructure of a shape memory alloy being heat treated and also mechanically deformed. From TLP: Superelasticity and Shape Memory Alloys Videos kindly donated by Vaclav Novak and Per Sittner Department of Functional Materials Institute of Physics of the ASCR, Prague Czech Republic |