Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Video Library Full Record for Video 10

Full Record for Video 10

Click to view video 10
[39 sec, audio: No]

View video in new window

Download
Windows media file [3692 Kb]
Quicktime video [2404 Kb]
video no
10
Brief description
Using a steel-aluminium bi-material strip, with the two constituent strips equally thick. The steel-aluminium strip is fixed securely in the tray, and liquid nitrogen carefully poured into the tray to estimate its boiling temperature. From TLP: Thermal expansion and the bi-material strip
Categories
Experimental procedure