[31 sec, audio: No]
View video in new window
Download
Windows media file [3255 Kb]
Quicktime video [5019 Kb]
- video no
- 113
- Brief description
- Phase transformation (20x magnification, 3x speed) for an isotropic liquid to chiral nematic liquid crystal. Although nucleation begins in a similar fashion to the regular nematic, we can see the different regions merge with one another to form the final ‘fingerprint structure’ that is characteristic of chiral nematics with their helical axis parallel to the surface of the slide. From TLP: Liquid Crystals
- Categories
- Optical microscopy
- Date
- 14/08/07
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International