Video Library
Browse the libraryAdvanced searchHelpAbout the video libraryTerms of useFeedback Print this page

Full Record for Video 133
[10 sec, audio: No]
View video in new window
Download
Windows media file [517 Kb]
Quicktime video [1678 Kb]
- video no
- 133
- Brief description
- The sample moves though θ (~5 to 45 °) while the detector scans though 2θ (~10 to 90 ° ). It has been speeded up as typical data collection time would be somewhere between 10 mins and 10 hours. From the TLP X-ray Diffraction Techniques
- Categories
- Experimental procedure
- Date
- 13/08/08
- Licence for re-use
DoITPoMS standard terms of use