Full Record for Video 139
[5 sec, audio: No]
View video in new window
Download
Windows media file [54 Kb]
Quicktime video [333 Kb]
- video no
- 139
- Brief description
- Cooper pairs. One ball makes a depression in the rubber sheet and moves on. A second ball rolls into the well and become effectively bound to the first ball. From the TLP Superconductivity
- Categories
- Atomistic animations
- Date
- 28/08/08
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International
You can also view this video on YouTube