Full Record for Video 180
[40 sec, audio: No]
View video in new window
Download
Windows media file [1323 Kb]
Quicktime video [701 Kb]
- video no
- 180
- Brief description
- Impact testing samples of various commercial chocolate bars. From TLP: Toughening