- video no
- 19
- Brief description
- Animation of slip by dislocation glide. Dislocation glide allows plastic deformation to occur at a much lower stress than would be required to move a whole plane of atoms past another. See also the bubble raft experiment (videos 17 and 18). From TLP Introduction to dislocations