Full Record for Video 2
[16 sec, audio: No]
View video in new window
Download
Windows media file [1461 Kb]
Quicktime video [904 Kb]
- video no
- 2
- Brief description
- A section of quartz cut perpendicular to the c-axis being heated from a point at its centre. A circle shows the thermal conductivity is the same in all directions in this plane. From Introduction to Anisotropy
- Categories
- Experimental procedure
- Date
- 02/08/06
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International