Full Record for Video 60
[66 sec, audio: No]
View video in new window
Download
Windows media file [6986 Kb]
Quicktime video [3708 Kb]
- video no
- 60
- Brief description
- Video demonstrating that the stiffness of rubber is proportional to temperature. The rubber is extended under a fixed load, and contracts when heated due to the increased stiffness, and therefore reduced strain. From TLP: The Stiffness of Rubber
- Categories
- Experimental procedure
- Date
- 09/08/06