Full Record for Video 80
[12 sec, audio: No]
View video in new window
Download
Windows media file [1304 Kb]
Quicktime video [1671 Kb]
- video no
- 80
- Brief description
- Heating a PET bottle over a bunsen burner flame. Before heating the plastic is in a less crystalline state than would be expected, as a result of the production process. Upon heating it recrystallises into a denser form, and therefore shrinks. (related topic - recycling polymers)
- Categories
- Experimental procedure
- Date
- 05/09/06