Categories > Metal or alloy > Keyword: steel

172 micrographs available, ordered by micrograph number.


Showing 11 - 20 of 172 micrographs Page 1 2 3 4 5 6 7 .. 18 | Previous | Next

Link to full record for micrograph 24 Micrograph 24 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 25 Micrograph 25 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 26 Micrograph 26 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 27 Micrograph 27 : Fe, C 0.9 (wt%), martensite
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 28 Micrograph 28 : Fe, C 0.9 (wt%), martensite
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 43 Micrograph 43 : Fe, C 0.2 (wt%), explosively deformed - mechanical twins
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 44 Micrograph 44 : Fe, C 0.2 (wt%), explosively deformed - mechanical twins
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 78 Micrograph 78 : Forging steel, brittle, intergranular fracture
System: Fe-C-X, Composition: Forging steel
Scanning electron microscopy (SEM)
800 μm
Link to full record for micrograph 133 Micrograph 133 : Steel, austenitised at 1200 centigrade for 120 s and then transformed isothermally at 350 centigrade for 2000 s before cooling to room temperature.
System: Fe-C-X, Composition: Fe, C 0.24, Si 2.18, Mn 2.32, Ni 1.05 (wt%)
Atomic force microscopy (AFM)
1 μm
Link to full record for micrograph 134 Micrograph 134 : High carbon steel
System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%)
Transmission electron microscopy (TEM)
600 nm