Browse the Library
Categories > Metal or alloy
708 micrographs available, ordered by micrograph number.
| Showing 21 - 30 of 708 micrographs | Page 1 2 3 4 5 6 7 .. 71 | Previous | Next |
![]() |
Micrograph
21
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
22
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
23
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Scanning electron microscopy (SEM) 50 μm |
![]() |
Micrograph
24
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Scanning electron microscopy (SEM) 10 μm |
![]() |
Micrograph
25
:
Fe, C 0.85 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 0.85 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
26
:
Fe, C 0.85 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 0.85 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
27
:
Fe, C 0.9 (wt%), martensite System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
28
:
Fe, C 0.9 (wt%), martensite System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Scanning electron microscopy (SEM) 10 μm |
![]() |
Micrograph
29
:
Cu 70, Zn 30 (wt%), annealed and cold rolled System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
30
:
Cu 70, Zn 30 (wt%), annealed and cold rolled System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 40 μm |