Browse the Library
Categories > Metal or alloy > Fe-C-X > Reflected light microscopy
268 micrographs available, ordered by micrograph number.
Showing 261 - 268 of 268 micrographs | Page 1 .. 21 22 23 24 25 26 27 | Previous | Next |
Micrograph
797
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
802
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
806
:
Austenitic stainless steel water quenched then cooled, showing transformation to g in the a lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Reflected light microscopy 50 μm |
|
Micrograph
819
:
Austenitic stainless steel water quenched then deformed in impact System: Fe-C-X, Composition: Stainless steel with Cr 13.7, Mn 14.2, C 0.12 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
833
:
Austenitic stainless steel solution treated, quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
854
:
Low Carbon Steel Grains, Copper Edge System: Fe-C-X, Composition: Fe, C low (wt%) Reflected light microscopy 500 μm |
|
Micrograph
935
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 2 mm |
Showing 261 - 268 of 268 micrographs | Page 1 .. 21 22 23 24 25 26 27 | Previous | Next |