Full Record for Micrograph 854
- Micrograph no
- 854
- Brief description
- Low Carbon Steel Grains, Copper Edge
- Keywords
- Categories
- System
- Fe-C-X
- Composition
- Fe, C low (wt%)
- Standard codes
- Reaction
- Processing
- Applications
- Sample preparation
- Technique
- Reflected light microscopy
- Length bar
- 500 μm
- Further information
- The edge of a 1p coin, showing a ferritic grain structure and a copper coating.
- Contributor
- Lewis Lea
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 12/08/10
- Licence for re-use
Attribution-Non-Commercial-Share Alike 2.0 UK: England & Wales