Micrograph no
857
Brief description
Low Carbon Steel
Keywords
Categories
System
Fe-C-X   Link to phase diagram
Composition
Fe, C low (wt%)
Standard codes
Reaction
Processing
Applications
Sample preparation
Technique
Atomic force microscopy (AFM)
Length bar
20 μm
Further information
The microstructure of ferritic steel in a 1p coin.