Categories > Metal or alloy > Fe-C-X > Reflected light microscopy
268 micrographs available, ordered by micrograph number.
Showing 41 - 50 of 268 micrographs | Page 1 2 3 4 5 6 7 8 .. 27 | Previous | Next |
Micrograph
215
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.08 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
216
:
Normalised carbon steel System: Fe-C-X, Composition: Fe, C 0.08 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
217
:
Low carbon steel normalised at 950°C System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 400 μm |
|
Micrograph
218
:
Low carbon steel normalised at 950°C System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 100 μm |
|
Micrograph
219
:
Low carbon steel from wood screw thread. System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 800 μm |
|
Micrograph
220
:
Low carbon steel from wood screw thread. System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 400 μm |
|
Micrograph
221
:
Low carbon steel from bottom of wood screw. System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 400 μm |
|
Micrograph
222
:
Low carbon steel from bottom of wood screw. System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 800 μm |
|
Micrograph
223
:
Annealed low carbon steel with carbides System: Fe-C-X, Composition: Fe, C low (wt%) Reflected light microscopy 400 μm |
|
Micrograph
224
:
Annealed low carbon steel with carbides System: Fe-C-X, Composition: Fe, C low (wt%) Reflected light microscopy 200 μm |