Full Record for Micrograph 221
[116 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 221
- Brief description
- Low carbon steel from bottom of wood screw.
- Keywords
- alloy
, carbon, iron, metal, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C very low (wt%)
- Standard codes
- Reaction
- Processing
- Rolled
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 400 μm
- Further information
- Low carbon steel. The resulting microstructure is therefore virtually all of the ferrite phase, since upon reaching the eutectoid temperature virtually all of the austenite will have transformed to ferrite. This sample is taken from the bottom of a wood screw, some directionality is observable due to the item being rolled.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs