Composition
6 micrographs for composition Fe, C very low (wt%), ordered by micrograph number.
![]() |
Micrograph
217
:
Low carbon steel normalised at 950°C System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
218
:
Low carbon steel normalised at 950°C System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
219
:
Low carbon steel from wood screw thread. System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
220
:
Low carbon steel from wood screw thread. System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
221
:
Low carbon steel from bottom of wood screw. System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
222
:
Low carbon steel from bottom of wood screw. System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 800 μm |