Full Record for Micrograph 218

[108 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr

- Micrograph no
- 218
- Brief description
- Low carbon steel normalised at 950°C
- Keywords
- alloy
, carbon, iron, metal, steel
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C very low (wt%)
- Standard codes
- Reaction
- Processing
- Normalised 950°C
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 100 μm
- Further information
- Wrought iron contains a very low amount of carbon. The resulting microstructure is therefore virtually all of the ferrite phase, since upon reaching the eutectoid temperature virtually all of the austenite will have transformed to ferrite. Some stringers of slag remain trapped in the solidified product.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
Attribution-Non-Commercial-Share Alike 2.0 UK: England & Wales