Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
802
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
806
:
Austenitic stainless steel water quenched then cooled, showing transformation to g in the a lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Reflected light microscopy 50 μm |
|
Micrograph
819
:
Austenitic stainless steel water quenched then deformed in impact System: Fe-C-X, Composition: Stainless steel with Cr 13.7, Mn 14.2, C 0.12 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
833
:
Austenitic stainless steel solution treated, quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
854
:
Low Carbon Steel Grains, Copper Edge System: Fe-C-X, Composition: Fe, C low (wt%) Reflected light microscopy 500 μm |
|
Micrograph
858
:
Bi 40wt%, Sn 60wt% System: Bi-Sn, Composition: Bi 40, Sn 60 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
859
:
Bi 60wt%, Sn 40wt% System: Bi-Sn, Composition: Bi 60, Sn 40 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
860
:
Bi 80wt%, Sn 20wt% System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
872
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
Showing 441 - 450 of 509 micrographs | Page 1 .. 42 43 44 45 46 47 48 .. 51 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.