Terracotta pottery System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 200 μm |
|
Micrograph
178
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 100 μm |
|
Micrograph
179
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 250 μm |
|
Micrograph
187
:
Part of a Denby pottery mug, showing the glaze on the surface System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
|
Micrograph
188
:
Part of a Denby pottery mug System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |