Browse the Library
Categories > Composite > Keyword: MMC
6 micrographs available, ordered by micrograph number.
![]() |
Micrograph
602
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (10 vol%) Reflected light microscopy, polarised 80 μm |
![]() |
Micrograph
603
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (5 vol%) Reflected light microscopy, polarised 80 μm |
![]() |
Micrograph
606
:
Extruded Saffil-containing metal matrix composite System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
610
:
Section of a metal matrix composite (MMC) System: Al, Composition: Commercial purity (99.5%) + 15 micron angular silicon carbide particles Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
611
:
Section of a metal matrix composite (MMC) after extrusion and annealing System: Al, Composition: Commercial purity (99.5%) + 13 micron alumina spheroids Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
616
:
Cavity formation in a tensile loaded alumina particulate composite System: Al, Composition: Commercial purity (99.5%) + 15 micron angular alumina particles Scanning electron microscopy (SEM) 80 μm |