578
:
Sprue in a sample of polypropylene (PP) System: Polypropylene (PP), Composition: Not specified Cross-polarised light microscopy 10 mm |
|
Micrograph
600
:
Spherulite in poly-3-hydroxy butyrate (PHB) System: Polyhydroxybutyrate (PHB), Composition: Not specified Cross-polarised light microscopy 1 μm |
|
Micrograph
601
:
Spherulites in in poly-3-hydroxy butyrate (PHB) System: Polyhydroxybutyrate (PHB), Composition: Not specified Cross-polarised light microscopy 240 nm |
|
Micrograph
612
:
Nematic liquid crystalline polymer System: Liquid crystalline polymer, Composition: K24 (4-cyano-4'-8-alkylbiphenyl) Cross-polarised light microscopy 100 μm |
|
Micrograph
637
:
Disclinations in a smectic LCP, revealed by decoration System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-7 Cross-polarised light microscopy 10 μm |
|
Micrograph
638
:
Disclinations in a smectic LCP, revealed by decoration System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-8 Cross-polarised light microscopy 10 μm |
Showing 11 - 16 of 16 micrographs | Page 1 2 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.