Showing 61 - 70 of 80 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next

Link to full record for micrograph 628 Micrograph 628 : Sintered salt (NaCl)
System: Na-Cl, Composition: Not specified
Scanning electron microscopy (SEM)
140 μm
Link to full record for micrograph 650 Micrograph 650 : Small ceramic pot showing centimetre scale crystals within the glaze
System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%)
Photography (no microscope)
20 mm
Link to full record for micrograph 655 Micrograph 655 : Small ceramic pot showing centimetre scale crystals within the glaze
System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%)
Photography (no microscope)
5 mm
Link to full record for micrograph 663 Micrograph 663 : Barium titanate ceramic
System: BaTiO3, Composition: Not specified
Reflected light microscopy
No length bar
Link to full record for micrograph 664 Micrograph 664 : Barium titanate ceramic
System: BaTiO3, Composition: Not specified
Reflected light microscopy
No length bar
Link to full record for micrograph 675 Micrograph 675 : Magnesia-Chromite Clinker
System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 676 Micrograph 676 : Magnesia-Chromite Clinker
System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 677 Micrograph 677 : Magnesia-Chromite Clinker
System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 678 Micrograph 678 : Magnesia-Chromite Clinker
System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 679 Micrograph 679 : BaO-Nd2O3-4TiO2
System: BaO-Nd2O3-4TiO2, Composition: Not specified
Reflected light microscopy
400 μm