Composition
6 micrographs for composition Cu 55, Zn 45 (wt%), ordered by micrograph number.
![]() |
Micrograph
449
:
Cu 55, Zn 45 (wt%) brass, rapidly cooled System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
450
:
Cu 55, Zn 45 (wt%) brass, rapidly cooled System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
451
:
Cu 55, Zn 45 (wt%) brass, rapidly cooled System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
455
:
Cu 55, Zn 45 (wt%) brass, as cast, dendritic System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
456
:
Cu 55, Zn 45 (wt%) brass, as cast, dendritic System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
457
:
Cu 55, Zn 45 (wt%) brass, as cast, dendritic System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 200 μm |