Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Contributor
44 micrographs contributed by Dr K M Knowles, ordered by micrograph number.
| Showing 11 - 20 of 44 micrographs | Page 1 2 3 4 5 | Previous | Next |
![]() |
Micrograph
170
:
ZnO varistor System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3 Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
171
:
ZnO varistor System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
172
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
173
:
Bone china, showing the glaze on the surface (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
174
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
175
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 100 μm |
![]() |
Micrograph
176
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 250 μm |
![]() |
Micrograph
177
:
Terracotta pottery System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 200 μm |
![]() |
Micrograph
178
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 100 μm |
![]() |
Micrograph
179
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 250 μm |
| Showing 11 - 20 of 44 micrographs | Page 1 2 3 4 5 | Previous | Next |