11 micrographs contributed by R J Mitchell, ordered by micrograph number.


Showing 1 - 10 of 11 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 724 Micrograph 724 : Ni-Superalloy, as-extruded microstructure
System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
10 μm
Link to full record for micrograph 725 Micrograph 725 : Ni-Superalloy, as-extruded microstructure
System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
10 μm
Link to full record for micrograph 726 Micrograph 726 : Ni-Superalloy, heat treated above gamma-prime solvus
System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
10 μm
Link to full record for micrograph 727 Micrograph 727 : Ni-Superalloy, heat treated above gamma-prime solvus
System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy)
Field emission gun scanning electron microscopy (FEGSEM) in secondary electron imaging (SEI) mode
100 nm
Link to full record for micrograph 728 Micrograph 728 : Ni-Superalloy, heat treated above gamma-prime solvus
System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
10 μm
Link to full record for micrograph 729 Micrograph 729 : Ni-Superalloy, exposed microstructure
System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
10 μm
Link to full record for micrograph 730 Micrograph 730 : Magnesium alloy
System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
200 μm
Link to full record for micrograph 731 Micrograph 731 : Metal matrix composite of magnesium and alumina fibres
System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy), reinforced with Alumina fibres with a volume fraction of 14%
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
10 μm
Link to full record for micrograph 732 Micrograph 732 : Magnesium alloy
System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
200 μm
Link to full record for micrograph 733 Micrograph 733 : Magnesium alloy, fracture surface
System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
20 μm