Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Contributor
11 micrographs contributed by R J Mitchell, ordered by micrograph number.
| Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
724
:
Ni-Superalloy, as-extruded microstructure System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
725
:
Ni-Superalloy, as-extruded microstructure System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
726
:
Ni-Superalloy, heat treated above gamma-prime solvus System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
727
:
Ni-Superalloy, heat treated above gamma-prime solvus System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Field emission gun scanning electron microscopy (FEGSEM) in secondary electron imaging (SEI) mode 100 nm |
![]() |
Micrograph
728
:
Ni-Superalloy, heat treated above gamma-prime solvus System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
729
:
Ni-Superalloy, exposed microstructure System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
730
:
Magnesium alloy System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 200 μm |
![]() |
Micrograph
731
:
Metal matrix composite of magnesium and alumina fibres System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy), reinforced with Alumina fibres with a volume fraction of 14% Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
732
:
Magnesium alloy System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 200 μm |
![]() |
Micrograph
733
:
Magnesium alloy, fracture surface System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 20 μm |
| Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |