Full Record for Micrograph 299
[138 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 299
- Brief description
- Fe, C 0.75 (wt%) steel, quenched, martensitic and manganese sulphides
- Keywords
- alloy
, carbon, iron, martensite
, metal, quenching
, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.75 (wt%)
- Standard codes
- Reaction
- Processing
- Quenched
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 200 μm
- Further information
- This steel has been quenched to produce martensite. Manganese has been added to remove sulphur from the alloy, and during solidification some of the MnS has been trapped and incorporated into the resultant product.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02