58 micrographs for keyword composite material, ordered by micrograph number.
| Showing 41 - 50 of 58 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
![]() |
Micrograph
622
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
623
:
Space-filling fire-resistant composite Barrikade (R) System: Barrikade, Composition: Expanded vermiculite, cured in ZnO and mixed with binder Photography (no microscope) 10 mm |
![]() |
Micrograph
624
:
Inter-particle bond in the fire-resistant composite Barrikade (R) System: Barrikade, Composition: Expanded vermiculite, cured in ZnO and mixed with binder Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 100 μm |
![]() |
Micrograph
626
:
Glass fibre reinforced thermoplastic matrix composite System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre Scanning electron microscopy (SEM) 60 μm |
![]() |
Micrograph
627
:
Glass fibre reinforced thermoplastic matrix composite System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
629
:
FORMGRIP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
630
:
FOAMCARP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
631
:
Coarse open celled aluminium foam produced by infiltration of sintered salt (FOAM-U-LIKE) System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
632
:
Open-celled aluminium foam System: Al, Composition: Not specified Photography (no microscope) 8 mm |
![]() |
Micrograph
633
:
Cross-section of an aluminium foam slab produced by gas injection System: Al, Composition: Not specified Photography (no microscope) 10 mm |