77 micrographs for keyword ceramic, ordered by micrograph number.
| Showing 21 - 30 of 77 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |
![]() |
Micrograph
173
:
Bone china, showing the glaze on the surface (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
174
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
175
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 100 μm |
![]() |
Micrograph
176
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 250 μm |
![]() |
Micrograph
177
:
Terracotta pottery System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 200 μm |
![]() |
Micrograph
178
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 100 μm |
![]() |
Micrograph
179
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 250 μm |
![]() |
Micrograph
180
:
Oven-to-tableware showing the glaze on the surface, using a sensitive tint plate System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 200 μm |
![]() |
Micrograph
181
:
Oven-to-tableware System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
182
:
Oven-to-tableware System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy 100 μm |
| Showing 21 - 30 of 77 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |