Micrograph
572
:
Birefringence in a film of polypropylene System: Polypropylene (PP), Composition: Not specified Cross-polarised light microscopy 10 mm |
![]() |
Micrograph
573
:
Birefringence in a film of polyethylene System: Low density polyethylene (LDPE), Composition: Not specified Cross-polarised light microscopy 14 mm |
![]() |
Micrograph
604
:
Extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
606
:
Extruded Saffil-containing metal matrix composite System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
608
:
Channelling contrast TEM image of subgrains of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Transmission electron microscopy (TEM) 600 nm |
![]() |
Micrograph
609
:
The grain structure of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
610
:
Section of a metal matrix composite (MMC) System: Al, Composition: Commercial purity (99.5%) + 15 micron angular silicon carbide particles Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
611
:
Section of a metal matrix composite (MMC) after extrusion and annealing System: Al, Composition: Commercial purity (99.5%) + 13 micron alumina spheroids Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
616
:
Cavity formation in a tensile loaded alumina particulate composite System: Al, Composition: Commercial purity (99.5%) + 15 micron angular alumina particles Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
724
:
Ni-Superalloy, as-extruded microstructure System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |