Link to full record for micrograph 21 Micrograph 21 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 22 Micrograph 22 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 23 Micrograph 23 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Scanning electron microscopy (SEM)
50 μm
Link to full record for micrograph 24 Micrograph 24 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 25 Micrograph 25 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 26 Micrograph 26 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 27 Micrograph 27 : Fe, C 0.9 (wt%), martensite
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 28 Micrograph 28 : Fe, C 0.9 (wt%), martensite
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 29 Micrograph 29 : Cu 70, Zn 30 (wt%), annealed and cold rolled
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 30 Micrograph 30 : Cu 70, Zn 30 (wt%), annealed and cold rolled
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
40 μm

Showing 21 - 30 of 535 micrographs Page 1 2 3 4 5 6 7 .. 54 | Previous | Next