Keyword
185 micrographs for keyword copper, ordered by micrograph number.
| Showing 61 - 70 of 185 micrographs | Page 1 .. 4 5 6 7 8 9 10 .. 19 | Previous | Next |
![]() |
Micrograph
447
:
Cu 65, Zn 35 (wt%) B4 brass, chill cast System: Cu-Zn, Composition: Cu 65, Zn 35 (wt%) (pure) Reflected light microscopy 400 μm |
![]() |
Micrograph
448
:
Cu 65, Zn 35 (wt%) B4 brass, chill cast System: Cu-Zn, Composition: Cu 65, Zn 35 (wt%) (pure) Reflected light microscopy 200 μm |
![]() |
Micrograph
449
:
Cu 55, Zn 45 (wt%) brass, rapidly cooled System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
450
:
Cu 55, Zn 45 (wt%) brass, rapidly cooled System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
451
:
Cu 55, Zn 45 (wt%) brass, rapidly cooled System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
452
:
Cu 52.5, Zn 47.5 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 52.5, Zn 47.5 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
453
:
Cu 52.5, Zn 47.5 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 52.5, Zn 47.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
454
:
Cu 52.5, Zn 47.5 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 52.5, Zn 47.5 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
455
:
Cu 55, Zn 45 (wt%) brass, as cast, dendritic System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
456
:
Cu 55, Zn 45 (wt%) brass, as cast, dendritic System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 400 μm |
| Showing 61 - 70 of 185 micrographs | Page 1 .. 4 5 6 7 8 9 10 .. 19 | Previous | Next |