- Brief description
- HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
- Keywords
- alloy
, brittle
, fracture
, intergranular
, metal, steel
- Categories
- Fracture, Metal or alloy
- System
- Fe-C-X
- Composition
- Not specified
- Standard codes
- Reaction
- Processing
- Applications
- Sample preparation
- Technique
- Scanning electron microscopy (SEM)
- Length bar
- 200 μm
- Further information
- Contributor
- S Munday
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 24/01/02