Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 196 and full record
- Micrograph no
- 196
- Brief description
- Tetragonal Zirconia Polycrystals (TZP)
- Keywords
- ceramic
, engineering ceramic, tough ceramic, toughness
, zirconia - Categories
- Ceramic
- System
- ZrO2-Y2O3
- Composition
- Y2O3 2-3, ZrO2 96-97 (wt%)
- Standard codes
- Reaction
- Processing
- Pressed powder mixtures sintered at 1400-1550ºC.
- Applications
- Where toughness, wear-resistance and refractoriness are needed e.g. extrusion dies, machinery wear parts and piston caps.
- Sample preparation
- Grind, polish, ion thin and carbon coat.
- Technique
- Bright-field TEM
- Length bar
- 600 nm
- Further information
- The comparatively low sintering temperature allows very fine grained (sub-micron), dense and so high strength as well as tough ceramics to be produced. The microstructure shows equiaxed, fine grains with little evidence of weakening grain boundary phases. Such microstructures have some of the highest values of toughness achieved in ceramics.
- Contributor
- Prof W E Lee
- Organisation
- Department of Engineering Materials, University of Sheffield
- Date
- 02/09/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International
View image alone .. in a new window
Help is available on downloading images