Micrograph 316 and full record
- Micrograph no
- 316
- Brief description
- Fe, C 0.9 (wt%) steel, hypereutectoid, quenched
- Keywords
- alloy
, carbon, iron, martensite
, metal, quenching
, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.9 (wt%)
- Standard codes
- Reaction
- Processing
- Quenched
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 400 μm
- Further information
- A high carbon steel that has been quenched producing martensite laths in the microstructure. High carbon steels are more prone to the formation of martensite since more excess carbon is available to be trapped interstitially.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs
- Micrograph 313: Fe, C 0.9 (wt%) steel, hypereutectoid, quenched and tempered (400 μm)
- Micrograph 314: Fe, C 0.9 (wt%) steel, hypereutectoid, quenched and tempered (200 μm)
- Micrograph 315: Fe, C 0.9 (wt%) steel, hypereutectoid, quenched and tempered (100 μm)
- Micrograph 317: Fe, C 0.9 (wt%) steel, hypereutectoid, quenched (200 μm)
- Micrograph 318: Fe, C 0.9 (wt%) steel, hypereutectoid, quenched (100 μm)
View image alone .. in a new window
Help is available on downloading images