Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 345 and full record
- Micrograph no
- 345
- Brief description
- Medium carbon, low alloy steel, isothermally transformed
- Keywords
- alloy
, carbon, iron, martensite
, metal, quenching
, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%)
- Standard codes
- BS 640M40, formerly En 111
- Reaction
- Processing
- Isothermal transform 450 ºC, 20s
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 100 μm
- Further information
- A medium carbon steel that has been quenched producing martensite laths in the microstructure. A tempering operation has been carried out in order to reduce the hardness of the metal.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International
View image alone .. in a new window
Help is available on downloading images