Micrograph 349 and full record
- Micrograph no
- 349
- Brief description
- Fe, C 1.35 (wt%) steel, hypereutectoid, quenched
- Keywords
- alloy
, carbon, iron, martensite
, metal, quenching
, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 1.35 (wt%)
- Standard codes
- Reaction
- Processing
- Austenitised at 1000 ºC, quenched into molten salt at 600 ºC , partially transformed, quenched into water at 200 ºC
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 200 μm
- Further information
- Centre
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02