Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 405 and full record
- Micrograph no
- 405
- Brief description
- Cast iron with magnesium induced spheroidised graphite
- Keywords
- alloy
, carbon, cast iron
, iron, manganese, metal - Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 2-4, other constituents (wt% typical) (Cast iron)
- Standard codes
- Reaction
- Processing
- Cast
- Applications
- Sample preparation
- Nital
- Technique
- Reflected light microscopy
- Length bar
- 100 μm
- Further information
- Cast iron is a brittle material and it is advantageous to process it in such a way to improve its ductility. The brittleness is partially due to the graphite flakes which act as nucleation sites for cracks. Therefore it is an advantage to have the graphite present as spheres. This can be achieved by a heat treatment regime or by the addition of a small amount of Mg which poisons the graphite growth directions.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs
- Micrograph 393: Cast iron with magnesium induced spheroidised graphite (400 μm)
- Micrograph 394: Cast iron with magnesium induced spheroidised graphite (200 μm)
- Micrograph 395: Cast iron with magnesium induced spheroidised graphite (100 μm)
- Micrograph 396: Cast iron with magnesium induced spheroidised graphite (400 μm)
- Micrograph 397: Cast iron with magnesium induced spheroidised graphite (400 μm)
- Micrograph 398: Cast iron with magnesium induced spheroidised graphite (200 μm)
- Micrograph 399: Cast iron with magnesium induced spheroidised graphite (100 μm)
- Micrograph 400: Cast iron with magnesium induced spheroidised graphite (400 μm)
- Micrograph 401: Cast iron with magnesium induced spheroidised graphite (100 μm)
- Micrograph 402: Cast iron with magnesium induced spheroidised graphite (100 μm)
- Micrograph 403: Cast iron with magnesium induced spheroidised graphite (400 μm)
- Micrograph 404: Cast iron with magnesium induced spheroidised graphite (200 μm)