- Brief description
- Beach marks on a polystyrene fracture surface
- Keywords
- beach marks
, fracture
, polymer
, polystyrene (PS) - Categories
- Fracture, Polymer
- System
- Polystyrene (PS)
- Composition
- Not specified
- Standard codes
- Reaction
- Processing
- Applications
- Polystyrene is hard and inexpensive and its use is very widespread. CD cases and clear plastic cups are common examples. Domestic appliance casings are also typically made from PS
- Sample preparation
- The surface has been sputter-coated with gold, to give a conducting surface
- Technique
- Scanning electron microscopy (SEM)
- Length bar
- 50 μm
- Further information
- The fracture surfaces are generally very sharp and angular, indicating fast, brittle fracture with little ductile tearing. 'Beach marks', can be seen where the fracture has grown at a speed comparable to the speed of sound in the material. This results in periodic, momentary arrests in the crack propagation and periodic ridges in the fracture surface as it advances. There is also evidence of the fracture surface branching onto different planes as it progresses.
- Contributor
- J A Curran
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 03/10/02