Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 723 and full record
- Micrograph no
- 723
- Brief description
- Ni-Superalloy
- Keywords
- creep
, nickel, single crystal - Categories
- Metal or alloy
- System
- Ni-X
- Composition
- Ni, Al, Re, W, Ta, Cr, Co, Ru (Ni-Superalloy)
- Standard codes
- Reaction
- Processing
- Solution heat treated, creep test
- Applications
- The material is in single crystal form for turbine blade application, the operation temperature could easily reach above 1200°C during flight cycles. So, the alloy needs to have good high temperature creep resistance and microstructural stability.
- Sample preparation
- Standard TEM preparation procedure
- Technique
- Transmission electron microscopy (TEM)
- Length bar
- 200 nm
- Further information
- (TBBF) two-beam condition was set near <001> to observe the dislocation structure in the crept Ni-base superalloy.
- Contributor
- A C Yeh
- Organisation
- Rolls-Royce University Technology Centre, Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 05/03/03
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs