Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 790 and full record
- Micrograph no
- 790
- Brief description
- Austempered ductile cast iron
- Keywords
- alloy
, austempering
, carbon, cast iron
, copper, ductile
, ferrite
, graphite
, iron, manganese, metal, molybdenum, pearlite
, silicon 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
- Standard codes
- Reaction
- Processing
- Applications
- Sample preparation
- Etchant: Nital 2%
- Technique
- Reflected light microscopy
- Length bar
- 20 μm
- Further information
- Austenitised at 950°C, austempered at 350°C for 64 min.
Source: http://www.msm.cam.ac.uk/phase-trans/2001/adi/adimore.html. - Contributor
- Dr M A Yescas-Gonzalez
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 18/07/03
- Licence for re-use
DoITPoMS standard terms of use- Related micrographs
- Micrograph 782: Austempered ductile cast iron (100 μm)
- Micrograph 783: Austempered ductile cast iron (100 μm)
- Micrograph 784: Austempered ductile cast iron (100 μm)
- Micrograph 785: Austempered ductile cast iron (20 μm)
- Micrograph 786: Austempered ductile cast iron (100 μm)
- Micrograph 787: Austempered ductile cast iron (20 μm)
- Micrograph 788: Austempered ductile cast iron (100 μm)
- Micrograph 789: Austempered ductile cast iron (40 μm)
- Micrograph 791: Austempered ductile cast iron (100 μm)
- Micrograph 792: Austempered ductile cast iron (20 μm)
- Micrograph 793: Austempered ductile cast iron (100 μm)
- Micrograph 794: Austempered ductile cast iron (20 μm)
View image alone .. in a new window
Help is available on downloading images