Micrograph 796 and full record
- Micrograph no
- 796
- Brief description
- Blackheart cast iron
- Keywords
- alloy
, blackheart cast iron
, carbon, cast iron
, ductile
, equiaxed
, graphite
, iron, metal - Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Blackheart cast iron
- Standard codes
- Reaction
- Processing
- Applications
- Sample preparation
- Etchant: Nital 2%
- Technique
- Reflected light microscopy
- Length bar
- 100 μm
- Further information
Source: http://www.msm.cam.ac.uk/phase-trans/2001/adi/cast.iron.html.- Contributor
- Dr M A Yescas-Gonzalez
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 18/07/03
- Licence for re-use
DoITPoMS standard terms of use- Related micrographs