Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 803 and full record
- Micrograph no
- 803
- Brief description
- Austenitic stainless steel solution treated, water quenched then tempered
- Keywords
- austenite
, stainless steel - Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
- Standard codes
- Reaction
- Processing
- Solution treated 12 hours at 1250ºC, water quenched then tempered 24 hours at 700ºC
- Applications
- Sample preparation
- Thin film
- Technique
- Transmission electron microscopy (TEM)
- Length bar
- 1 μm
- Further information
- Contributor
- Professor Sir R W K Honeycombe
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 07/01/04
- Licence for re-use
DoITPoMS standard terms of use
View image alone .. in a new window