Micrograph 850 and full record
- Micrograph no
- 850
- Brief description
- Stainless Steel 430.
- Keywords
- steel
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Stainless steel 430
- Standard codes
- Reaction
- Processing
- Laser micromachining
- Applications
- Sample preparation
- Technique
- Atomic force microscopy (AFM)
- Length bar
- 20 μm
- Further information
- Grooves produced by a laser micromachining process in stainless steel 430.
- Contributor
- Jorge Sorbal
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 12/08/10
- Licence for re-use
- Attribution-NonCommercial-ShareAlike 4.0 International
View image alone .. in a new window
Help is available on downloading images