Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

System
21 micrographs for system Al, ordered by micrograph number.
| Showing 1 - 10 of 21 micrographs | Page 1 2 3 | Previous | Next |
![]() |
Micrograph
82
:
Aluminium, fracture surface System: Al, Composition: Not specified Scanning electron microscopy (SEM) 15 μm |
![]() |
Micrograph
83
:
Aluminium, fracture surface System: Al, Composition: Not specified Scanning electron microscopy (SEM) 50 μm |
![]() |
Micrograph
604
:
Extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
605
:
Fracture surface formed by hot tearing (solidification cracking) System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
606
:
Extruded Saffil-containing metal matrix composite System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
607
:
Fibre fracture in a metal matrix composite System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
608
:
Channelling contrast TEM image of subgrains of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Transmission electron microscopy (TEM) 600 nm |
![]() |
Micrograph
609
:
The grain structure of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
610
:
Section of a metal matrix composite (MMC) System: Al, Composition: Commercial purity (99.5%) + 15 micron angular silicon carbide particles Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
611
:
Section of a metal matrix composite (MMC) after extrusion and annealing System: Al, Composition: Commercial purity (99.5%) + 13 micron alumina spheroids Reflected light microscopy, polarised 40 μm |
| Showing 1 - 10 of 21 micrographs | Page 1 2 3 | Previous | Next |