AimsBefore you startIntroductionBasic conceptDemonstration of projectionImportant properties of the stereographic projectionThe Wulff netUse of the Wulff net in constructing a stereogramPlotting poles on the stereogram through use of the Wulff netIdentifying poles on a stereogram through use of the Wulff netApplications of the Stereographic Projection - SlipInteractive Wulff netSummaryQuestionsGoing furtherTLP creditsTLP contentsShow all contentViewing and downloading resourcesAbout the TLPsTerms of useFeedbackCredits Print this page
PreviousNext
Plotting poles on the stereogram through use of the Wulff net
It is possible to make use of the Wulff net to find the angular relationships of various poles of planes. However, to find these angular relationships, we need to plot the poles onto a Wulff net. There are various ways of doing this, described below.