- Brief description
- Slip proceeding on previously deformed single cadmium crystal. An unusually large slip step can be seen on the left-hand edge of the specimen. As slip proceeds, the slip planes rotate towards the tensile axis, but the large slip step does not increase in size. From TLP: Slip in Single Crystals